Usually used for welding chromium-nickel stainless steel base metals of similar composition stabilized with either Nb or Ti. Although Nb is the stabilizing element usually specified in Type 347 alloys, it should be recognized that tantalum (Ta) is also present.
Ta and Nb are almost equally effective in stabilizing carbon and in providing high-temperature strength. If dilution by the base metal produces a low ferrite or fully austenitic weld metal, the crack sensitivity of the weld may increase substantially.
Additional Information |
---|
Packaging Description:10lb tube |
Weld Process:TIG |
AWS Spec :ER410 |
Packaging:10lb tube |
Grade:410 |
Diameter:1.6mm |
Polarity:DC+ |
Brand:Exocor |